●High hardness●Toughness●High bending strength● High wear resistance ● Low friction coefficient ● Strong corrosion resistance ● Low thermal expansion coefficient ● High density ● Highest thermal conductivity
Silicon nitride has a low self diffusion coefficient, strong resistance to impurity diffusion and waterproof vapor penetration; Silicon nitride has excellent properties such as corrosion resistance, oxidation resistance, friction resistance, and self-lubrication; Silicon nitride does not react with molten silicon Si and does not adhere to Si melt, exhibiting excellent corrosion resistance and detachment. The thermal conductivity of silicon nitride crucibles is several tens of times higher than that of quartz crucibles. Using high-purity and high thermal conductivity silicon nitride crucibles instead of quartz crucibles can significantly compress the melting time and furnace cooling time when drawing monocrystalline silicon. This not only improves production efficiency, but also reduces electricity consumption, saving energy and production operating costs.
1. Self developed and self prepared silicon nitride powder
2. Dry pressing and isostatic pressing forming
3. Gas pressure sintering
4. Precision machining: flat grinding, outer diameter/inner diameter grinding, precision machining, grinding, polishing and grinding
5. Strict testing
● New energy ● Medical ● Electricity ● Petroleum ● Chemical engineering ● Aerospace ● Military industry ● Electronics ● Semiconductor manufacturing components, etc.
Name/Characteristics | alumina | Zirconia | silicon nitride | Aluminum nitride | silicon carbide | boron nitride |
appearance | White or milky white or ivory | ivory | dark gray | brown | black | white |
density | 3.9 | 6.05 | 3.2 | 3.3 | 3.15 | 2.3 |
permittivity | 10 | 30 | 11 | 8 | 9.6 | 3.1 |
Thermal conductivity W/mk | 20~37 | 5-8 | 90-130 | 90~230 | 25-40 | 33 |
Thermal expansion coefficient(Negative sixth power of ten/K) | 4.5~8 (Negative sixth power of ten/K) |
8~11.5 (Negative sixth power of ten/K) |
3.2 (Negative sixth power of ten/K) |
4.5 (Negative sixth power of ten/K) |
4.8-5.2 (Negative sixth power of ten/K) |
15 (Negative sixth power of ten/K) |
Elastic modulus(Gpa) | 380 | 210 | 300~320 | 320 | 400~420 | * |
Poisson's ratio | 0.27 | 0.3 | 0.26 | 0.25 | 0.19 | * |
High temperature resistance | 500°~1700° | 500°~1700° | 800°~1300° | 1700° | 1700° | 2200° |
Acid and alkali corrosion resistance | strong | strong | strong | strong | strong | same as |
magnetism | not have | not have | not have | not have | not have | not have |
dimensional stability | Little change with temperature | Little change with temperature | Little change with temperature | Little change with temperature | Little change with temperature | Little change with temperature |
thermal shock resistance△T.℃ | 200 | 400 | 800 | 400 | 600 | * |
Operating centrifugal force | medium | more | small | small | small | small |
By product
Application requirement
Design and research
Optimization scheme
Strict essence
Precision drawing
piggyback
Select ingredients
Multiple forming
Fired blank
Grinding and polishing
Precision machining
Multiple gage
Professional survey
Qualified product
Package and ship
Dongguan Zhongli Nano Ceramics Technology Co., Ltd. © Copyright 2023